    8. Heat treatment

    After hot forming and processing, the final touch is to obtain the right microstructure, which determines the final properties:

    • grain size ;

    • the distribution and size of the desired precipitates (essentially the hardening phases).

    Heat treatment generally consists of three major stages [M 1 165] :

    • solution heat treatment (950/1,200°C) ;

    • cooling mode after dissolving: air, oil, water ;

    • ...
    You do not have access to this resource.

    Exclusive to subscribers. 97% yet to be discovered!

    You do not have access to this resource.
    Click here to request your free trial access!

    Already subscribed? Log in!


    The Ultimate Scientific and Technical Reference

    A Comprehensive Knowledge Base, with over 1,200 authors and 100 scientific advisors
    + More than 10,000 articles and 1,000 how-to sheets, over 800 new or updated articles every year
    From design to prototyping, right through to industrialization, the reference for securing the development of your industrial projects

    This article is included in

    Functional materials - Bio-based materials

    This offer includes:

    Knowledge Base

    Updated and enriched with articles validated by our scientific committees

    Services

    A set of exclusive tools to complement the resources

    Practical Path

    Operational and didactic, to guarantee the acquisition of transversal skills

    Doc & Quiz

    Interactive articles with quizzes, for constructive reading

    Subscribe now!

    Ongoing reading
    Heat treatment
    Outline