ABSTRACT

This article looks at the genesis of residual stresses during the induction hardening process. After a short presentation of induction technology, the experimental protocol is described. The description of the “mechanical hardenability” concept and the “thermal-kinetic” effect will show the importance of quenching velocity for the residual stresses generated after the surface hardening heat treatments. The appraisal of residual stresses is necessary to estimate the sensitivity of quenching cracks for the different induction hardening steels.

Read this article from a comprehensive knowledge base, updated and supplemented with articles reviewed by scientific committees.

Read the article

AUTHOR

 INTRODUCTION

In the same way as thermochemical treatments, surface induction heating followed by quenching generates a field of residual compressive stresses which, among other things, improves the fatigue life of the treated product.

Taking an interest in residual stresses during surface heating also means gaining a better understanding of tapping phenomena and the indications associated with the deformations caused by heat treatment.

Based on several scientific studies, the aim of this article is to understand the mechanisms involved in the generation of residual stresses during martensitic hardening following surface induction heating.

After a brief introduction to induction heating, which will describe the experimental protocol that led to the results you are about to see, the second section will be devoted to understanding the genesis of residual stresses in our case. It will review various concepts specific to residual stresses: mechanical hardenability and the thermo-kinetic approach associated with thermal gradients and transformation gradients at the origin of the generation of residual stresses in induction.

We will then discuss the impact of carbon percentage on X-ray diffraction results when estimating residual stresses using the Ψ 2 method.

Key points

Area: Surface induction heating

Degree of technology dissemination: Maturity

Technologies involved: Surface induction heating

Applications: Automotive

Contact: [email protected] / http://www.metallocorner.fr

You do not have access to this resource.

Exclusive to subscribers. 97% yet to be discovered!

You do not have access to this resource.
Click here to request your free trial access!

Already subscribed? Log in!


The Ultimate Scientific and Technical Reference

A Comprehensive Knowledge Base, with over 1,200 authors and 100 scientific advisors
+ More than 10,000 articles and 1,000 how-to sheets, over 800 new or updated articles every year
From design to prototyping, right through to industrialization, the reference for securing the development of your industrial projects

KEYWORDS

quenching   |   residual stresses   |   induction   |   surface hardening


This article is included in

Technological innovations

This offer includes:

Knowledge Base

Updated and enriched with articles validated by our scientific committees

Services

A set of exclusive tools to complement the resources

Practical Path

Operational and didactic, to guarantee the acquisition of transversal skills

Doc & Quiz

Interactive articles with quizzes, for constructive reading

Subscribe now!

Ongoing reading
Residual stresses after surface induction treatment