2.1 Influence of deposit control parameters
As a general rule, a decrease in pH leads to a lowering of cathodic efficiencies. The pH varies as a result of the cathodic and anodic reactions occurring during electrolysis, and excessive deviations can lead to the formation of hydroxides (see § ...
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
The Ultimate Scientific and Technical Reference
This article is included in
Metal treatments
This offer includes:
Knowledge Base
Updated and enriched with articles validated by our scientific committees
Services
A set of exclusive tools to complement the resources
Practical Path
Operational and didactic, to guarantee the acquisition of transversal skills
Doc & Quiz
Interactive articles with quizzes, for constructive reading
Maintenance and inspection
References
Suppliers (products and/or materials)
(non-exhaustive list)
ATOTECH France
AMPERE INDUSTRIE
BAYER SA
CAPOL Processes
CHAMPOISEAU SA
CORELEC (Sté)
COVENTYA SAS
ELECTRO FINISH (Company)
ENGELHARD CLAL
...
French organizations
CEFRACOR: French Anticorrosion Centre
C.E.M.: Cercle d'Études des Métaux (Metal Study Circle)
CETIM: Technical Center for Mechanical Industries
IFETS: Institut Français de l'Environnement et des Traitements de Surface (French Institute for the Environment and Surface Treatments)
S.A.T.S.: Syndicat National des Entreprises...
Standardization
Association française de normalisation AFNOR
- Méthodes d'essai de corrosion des revêtements métalliques et inorganiques sur substrats métalliques. Cotation des éprouvettes et des articles manufacturés soumis aux essais de corrosion (NF A91-023). - NF EN ISO 10289 - Avr. 2001
- Metal corrosion protection – Electrolytic coatings of nickel, nickel plus chromium, copper plus nickel and copper plus nickel plus chromium...
Regulations
At the time of writing, the use of nickel solutions and their release into the environment in surface treatment plants are subject to the regulations set out in the decree of September 26, 1985 (published in the Journal Officiel of November 16, 1985). This decree defines the maximum permissible concentration of various constituents, such as metal ions (chromium, copper, iron, zinc, cadmium, etc.) and other components (cyanides,...
Websites
To find out more about the toxicity of nickel and the measures to take to protect against the risks associated with the use of nickel and its salts, we recommend that you visit the INRS website. http://www.inrs.fr
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
The Ultimate Scientific and Technical Reference