8. Solidification structure
The solidification structure is entirely basaltic dendritic (figure 7 ), which is not the ideal structure. This is due to the cooling flows imposed by the rail ends, despite oxypropane preheating to 700°C at the surface.
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
![](/assets/images/logo-eti-286623ed91fa802ce039246e516e5852.png)
The Ultimate Scientific and Technical Reference
This article is included in
Material processing - Assembly
This offer includes:
Knowledge Base
Updated and enriched with articles validated by our scientific committees
Services
A set of exclusive tools to complement the resources
Practical Path
Operational and didactic, to guarantee the acquisition of transversal skills
Doc & Quiz
Interactive articles with quizzes, for constructive reading
Solidification structure
Bibliography
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
![](/assets/images/logo-eti-286623ed91fa802ce039246e516e5852.png)
The Ultimate Scientific and Technical Reference