12. Glossary
Billette; ticket
A bar made from an ingot processed by forging, rolling or extrusion, with a constant round or square cross-section.
Electrode; electrod
Generally cylindrical shape obtained after casting in a vacuum induction furnace, for remelting in a vacuum arc remelting or slag remelting furnace.
Vacuum induction furnace (VIF); Vacuum Induction Melting (VIM)
Vacuum induction melting process for adding highly oxidizable metallic elements with high yields.
Inclusions; inclusions
Particles of impurities or foreign matter present or introduced at any stage of alloy manufacture: oxides, nitrides, carbonitrides, etc.
Ségrégation; segregation
Product area with abnormal...
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
![](/assets/images/logo-eti-286623ed91fa802ce039246e516e5852.png)
The Ultimate Scientific and Technical Reference
This article is included in
Studies and properties of metals
This offer includes:
Knowledge Base
Updated and enriched with articles validated by our scientific committees
Services
A set of exclusive tools to complement the resources
Practical Path
Operational and didactic, to guarantee the acquisition of transversal skills
Doc & Quiz
Interactive articles with quizzes, for constructive reading
Glossary
Bibliography
Bibliography
Events
International Symposium on Superalloys. Seven Springs. USA. International conference on superalloys, held every 4 years. TMS (The minerals, Metals and Materials Society) http://www.tms.org
International Symposium on Superalloys 718 and Derivatives. Pittsburgh, USA. Conference on 718 superalloys and derivatives held every 4 years in the United...
Directory
Documentation – Training – Seminars (non-exhaustive list)
Proceedings of the International Symposium on Superalloys (Seven Springs) (1968-1972-1976-1980-1984-1988-1992-1996-2000-2004-2008-1012-2016- 2020)
Proceedings of the International symposium on superalloys 718 and Derivatives (1989-1991-1994-1997-2001-2005-2010-2014-2018)
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
![](/assets/images/logo-eti-286623ed91fa802ce039246e516e5852.png)
The Ultimate Scientific and Technical Reference