4. Mechanical properties
Table 2 summarizes the tensile and hardness characteristics of selected materials. The influence of sampling direction is particularly important for yield strength and elongation at break.
For thin pilger tubes used in nuclear applications (thickness around 0.5 mm), the Kearns factors are approximately f L = 0.06, f T = 0.34, f N = 0.60. For thicker products (e.g. extruded tube, hot-rolled sheet with a thickness of 6 mm), the transverse factor f T may be significantly higher, to the detriment of f N (f T = 0.50, f ...
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
The Ultimate Scientific and Technical Reference
This article is included in
Studies and properties of metals
This offer includes:
Knowledge Base
Updated and enriched with articles validated by our scientific committees
Services
A set of exclusive tools to complement the resources
Practical Path
Operational and didactic, to guarantee the acquisition of transversal skills
Doc & Quiz
Interactive articles with quizzes, for constructive reading
Mechanical properties
Bibliography
Norms and standards
Most standards for zirconium and hafnium metal products, or alloys, are American ASTM standards. A few French standards also exist. Few standards concern hafnium.
-
French standards
- Corrosion of metals and alloys – Aqueous corrosion testing of zirconium alloys used in nuclear reactors. - NF EN ISO 10270 - Juillet 2008
- Description and qualification...
Manufacturers – Suppliers – Distributors
Please refer in particular to manufacturers' websites:
France
-
Areva NP
United States
-
ATI Wah Chang
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!
The Ultimate Scientific and Technical Reference