2. Conducting experiments
The general shape of the signal and the transitions that can be associated with it have already been described (§ 1.3 ). The purpose of this section is to describe the correct experimental procedure.
2.1 Base lines
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!

The Ultimate Scientific and Technical Reference
This article is included in
Analysis and Characterization
This offer includes:
Knowledge Base
Updated and enriched with articles validated by our scientific committees
Services
A set of exclusive tools to complement the resources
Practical Path
Operational and didactic, to guarantee the acquisition of transversal skills
Doc & Quiz
Interactive articles with quizzes, for constructive reading
Conducting experiments
Bibliography
Standards and norms
The international standard ISO (International Standardisation Organisation) is recommended but not mandatory.
The European standard (EN) is mandatory. It replaces the equivalent national standard.
The French standard (NF) applies in the absence of other European or international standards.
Differential Scanning Calorimetry for plastics is covered...
Directory
Associations French Association for Calorimetry and Thermal Analysis http://www.afcat.org
International Conference for Thermal Analysis and Calorimetry http://www.ictac.org
Exclusive to subscribers. 97% yet to be discovered!
You do not have access to this resource.
Click here to request your free trial access!
Already subscribed? Log in!

The Ultimate Scientific and Technical Reference